3M 4412N

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

3M 4412N

Main features

  • 2.0 mm Sealing-Tape Thickness
  • Instantly Paintable Ionomer Backing
  • Immediate Seal Without Chemical Cure

Product Description

3M Extreme Sealing Tape 4412N is a translucent, single-coated acrylic sealing tape for covering existing joints, seams, and penetrations in metal and plastic assemblies. Its typical 2.0 mm total thickness comprises 1.9 mm adhesive and a 0.1 mm ionomer backing. Applied with pressure to clean surfaces, it seals immediately, while full bond strength generally develops after 24 hours. The ideal application range is 21 to 38 deg C, with a suggested minimum of 10 deg C. The abrasion-resistant backing is instantly paintable and accepts overlapping tape joints; overlaps should extend at least 2 cm.

Key features

  • 2.0 mm conformable construction: Typical thickness includes 1.9 mm acrylic adhesive and a 0.1 mm ionomer backing, excluding the liner.
  • Immediate sealing on contact: Pressure application establishes the seal before the bond generally reaches full strength after 24 hours.
  • Paintable ionomer backing: The flexible, abrasion-resistant surface can be painted immediately and supports tape-to-tape overlap joints.

Applications

Sealing existing joints, seams, and penetrations on metals, plastics, and other compatible surfaces.

Product Family

3M 4412N

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Translucent
DensityDensity
820 kg/m3
Total ThicknessTotal Thickness
2000 μm
Mechanical Properties
ElongationElongation
400 %
Tensile Strength (Thin Film)Tensile Strength (Thin Film)
23 N/cm
Other Properties
Storage TemperatureStorage Temperature
4-38 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Values are typical and not specifications.

PropertyValueUnitMethod / condition
Backing materialIonomer-Single-coated tape construction
Adhesive typeAcrylic-Pressure-sensitive sealing layer
Total thickness2.0 (80)mm (mil)Typical tape construction
Shelf life24monthsUnopened product under stated storage conditions

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers