Main features

  • Low-Temperature 155 to 190 deg C Reflow
  • Extended 8-Hour Stencil Life
  • Air or Nitrogen Reflow

Product Description

ALPHA CVP-520 Solder Paste is a low-melting-point, no-clean, lead-free solder paste for low-temperature surface-mount assembly. Available configurations include multiple Sn/Bi/Ag alloy options with Type 3, Type 4, or Type 5 powder. Low-temperature processing uses peak reflow profiles between 155 and 190 deg C, and stencil life is more than 8 hours at 23 deg C and 50% RH. The paste is compatible with clean-dry air or nitrogen reflow. In suitable assemblies with temperature-sensitive through-hole components, CVP-520 can eliminate an extra wave or selective soldering process step.

Key features

  • Configurable paste: Available alloy configurations are paired with Type 3, Type 4, or Type 5 powder options.
  • Extended stencil life: Stencil life is more than 8 hours at 23 deg C and 50% RH.
  • Low-temperature reflow: Peak reflow profiles between 155 and 190 deg C can be run in clean-dry air or nitrogen.

Applications

Low-temperature surface-mount soldering and reflow assembly.

Product Family

ALPHA CNP CVP520

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Chemical Properties
Melting PointMelting Point
Below 140°C

Additional Information

Technical properties

As-supplied and process properties

CVP-520 is offered in multiple alloy and powder configurations; exact processing details depend on the selected configuration.

PropertyValueUnitMethod / condition
Alloy options42Sn/57.6Bi/0.4Ag; 42Sn/58Bi; 42Sn/57Bi/1.0Ag on requestAvailable configurations
Powder typesType 3, Type 4, Type 5Available configurations
Stencil lifeMore than 8hours23 deg C; 50% RH
Refrigerated shelf life6months0 to 10 deg C
Stencil working temperature19 to 29deg CPrinting on stencil
Print speed40 to 100mm/secStandard and fine-pitch stencil printing
Peak reflow temperature155 to 190deg CGeneral effective range; configuration dependent
Reflow atmosphereAir or N2Clean-dry air or nitrogen

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers