ARALDITE DY026

Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations

ARALDITE DY026

Main features

  • 110 to 115 g/eq Epoxy Equivalent Weight
  • Difunctional Epoxy Reactive Diluent
  • Composite and Electrical Epoxy Formulations

Product Description

ARALDITE DY 026 is a clear, low-viscosity difunctional reactive diluent for epoxy resins used in composite and electrical formulations. It has an epoxy equivalent weight of 110 to 115 g/eq by ISO 3001, density of 1.08 g/cm^3 at 25 deg C, and viscosity of 11 to 15 mPa s at 25 deg C by ISO 12058-1. Flash point is at least 156 deg C by ISO 2719. The material is also used as an adhesion promoter and flexibilizer in epoxy formulations, including high-temperature epoxy adhesive formulations.

Key features

  • 110 to 115 g/eq epoxy equivalent: Epoxy equivalent weight is 110 to 115 g/eq by ISO 3001.
  • 11 to 15 mPa s viscosity: Low as-supplied viscosity is 11 to 15 mPa s at 25 deg C by ISO 12058-1.
  • Reactive formulation function: The difunctional diluent is used as an adhesion promoter and flexibilizer in epoxy formulations.

Applications

Epoxy formulation in composites, electrical applications, electrical components, and high-temperature epoxy adhesive formulations.

Product Family

ARALDITE DY026

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
clear liquid
Density (g)Density (g)
@25 °C, 1.08 g/cm3
Physical Properties
ViscosityViscosity
@25 °C, 11 - 15 mPa.s
Thermal Properties
Flash PointFlash Point
> 156 °C

Additional Information

Technical properties

As supplied

PropertyValueUnitMethod / condition
Physical formLiquidAs supplied
AppearanceClear liquidAs supplied
Epoxy equivalent weight110 to 115g/eqISO 3001
Density1.08g/cm^3ISO 1675; 25 deg C
Flash point>= 156deg CISO 2719
Viscosity11 to 15mPa sISO 12058-1; falling ball; 25 deg C
Shelf life2yearsStorage at 2 to 40 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers