BOSTIK 1200
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

Main features
- 25% Joint-Movement Capability
- 570% Cured Elongation
- 10-Minute Tooling Window
Product Description
Bostik 1200 Acetoxy Cure Silicone Sealant is a one-component moisture-curing silicone designed for perimeter and joint sealing on non-porous construction surfaces. It develops adhesion to glass, glazed ceramic tile, and aluminum and cures to a flexible elastomer with 570% elongation and +/-25% joint movement capability under the documented test conditions. A 10-minute tool/work time supports placement and tooling, while the cured service-temperature range extends from -45 to 150 deg C. Applications include sealing around windows and doors, metal frames, skylights, and selected dissimilar-material joints within the supported substrate scope.
Key features
- 25% Joint Movement: Demonstrates +/-25% joint movement capability under the documented joint-movement test.
- 570% Cured Elongation: Provides 570% elongation at break after the documented 14-day cure condition.
- 10-Minute Tooling Window: A 10-minute tool/work time supports placement and finishing before skin formation.
Applications
Perimeter sealing around windows and doors; sealing metal frames, windows and skylights; selected dissimilar-material joints within the documented substrate scope.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Tool / work time | 10 | min | Typical uncured property |
| Skin time | 25 | min | Typical uncured property |
| Flow / sag / slump | 0.1 | in | TT-S-001543A / ASTM C639 |
Final-state properties
Typical cured properties after 14 days at 77 deg F and 50% RH unless otherwise noted.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Hardness | 17 | Shore A | ASTM D2240 |
| Modulus at 100% | 58 | psi | ASTM D412 |
| Tensile strength at break | 290 | psi | ASTM D412 |
| Elongation at break | 570 | % | ASTM D412 |
| Joint movement capability | +/-25 | % | TT-S-001543A / ASTM C719 |
| Service temperature | -45 to 150 | deg C | Cured service range |