BOSTIK PA145
Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

Main features
- 141 deg C Dry-Heat Activation
- Resists Cleaning and Home Laundering
- Fabrics, Foam and Vinyl Bonding
Product Description
Bostik PA145 is a nonwoven polyamide web adhesive made in a fine-filament pattern and supplied in roll form for lamination. The web works in intermittent or continuous processes and may be activated by steam or dry heat. Dry-heat activation requires 141 deg C, while steam activation requires 110 deg C. PA145 bonds fabrics, urethane foam, and vinyls, resists repeated dry cleaning and home laundering, and is used for automotive upholstery, filter media, footwear, skin-to-core constructions, and apparel laminates.
Key features
- Steam or dry-heat activation: Dry heat activation at 141 deg C or steam activation at 110 deg C.
- Fine-filament roll web: Nonwoven roll format provides uniform adhesive coverage for intermittent or continuous processing.
- Cleaning-resistant bonds: Product resists repeated dry cleaning and home laundering in its textile-lamination use.
Applications
Automotive upholstery, filter media, footwear, skin-to-core, and apparel laminating.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Milky white nonwoven fabric | Typical physical property | |
| Basis weight range | 15 to 100 | g/yd^2 | Typical physical property |
| Trimmed width | 10 to 68 | in | Typical roll width |
| Typical roll length | 500 to 1000 | linear yd | Roll form; typical |
| Shelf life | Approximately 24 | months | Stored below 54 deg C |