Main features

  • Low-Viscosity Mold Release Application
  • 100% Solids Silicone System
  • 12-Month Shelf Life

Product Description

CONAP MR-5016 Mold Release Agent is a low-viscosity silicone-polymer liquid release and parting agent for potting, casting, and molding operations. The clear, 100% solids material has an approximate viscosity of 225 cP at 25 deg C and specific gravity of approximately 0.97. Its flash point is above 201 deg F, and the product has a 12-month shelf life under the stated storage conditions. Applications include release of epoxy, polyurethane, polyester, and other plastic or resin systems from non-porous molds, including simple and complex mold geometries.

Key features

  • Low-viscosity release: Approximate viscosity is 225 cP at 25 deg C for liquid mold-release application.
  • 100% solids silicone system: Clear silicone-polymer material with approximately 0.97 specific gravity.
  • 12-month shelf life: Shelf life is 12 months under the stated storage conditions.

Applications

Mold release for epoxy, polyurethane, polyester, and other plastic or resin systems from non-porous molds.

Product Family

CONATHANE MR-5016

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Clear
Specific GravitySpecific Gravity
0.97
Physical Properties
ViscosityViscosity
225 mPa.s
Thermal Properties
Flash PointFlash Point
>94 °C

Additional Information

Technical properties

As-supplied properties

PropertyValueUnitMethod / condition
AppearanceClearAs supplied
ViscosityApprox. 225cP25 deg C
Specific gravityApprox. 0.9725 deg C
Solids100%As supplied
Flash pointAbove 201deg FAs supplied
Shelf life12monthsStated storage conditions

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers