DOWSIL 7094
Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

Main features
- Self-Leveling Flowable Placement
- 400% Cured Elongation
- 25-Minute Skin-Over Time
Product Description
DOWSIL 7094 Flowable Sealant flows and self-levels into gaps where a one-part, neutral-cure silicone sealant is required for sealing or bonding. The black or white viscous liquid has a typical density of 1.30 g/cm^3 and viscosity of 28,000 mPa s, allowing flow into gaps and airless-spray application. At 23 deg C and 50% relative humidity, it skins in about 25 minutes, becomes tack-free in about 50 minutes and cures inward from the exposed surface. After seven days under those conditions, the sealant has Shore A 19 hardness, 400% elongation and 1.2 MPa tensile strength.
Key features
- Flowable self-leveling rheology: Typical viscosity is 28,000 mPa s for gap filling and spray application.
- 25-minute skin-over time: Supports tooling and assembly before surface cure.
- Flexible cured seal: Typical elongation is 400% with Shore A 19 hardness.
Applications
Sealing and bonding applications requiring a low-viscosity, self-leveling silicone sealant.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Additional Information
As-supplied / before-processing properties
Typical as-supplied and cure-development properties. Values are not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Black or white viscous liquid | As supplied | |
| Density | 1.30 | g/cm^3 | CTM0097B |
| Viscosity | 28000 | mPa s | CTM0050 |
| Skin-over time | 25 | min | CTM0098; 23 deg C and 50% RH |
| Tack-free time | 50 | min | CTM0095A; 23 deg C and 50% RH |
| Cure depth | About 2 | mm | After 24 hr at room temperature and 50% RH |
| Shelf life | 12 | months | Below 30 deg C in original unopened container |
After-processing / final-state properties
Typical mechanical properties after seven days in air at 23 deg C and 50% relative humidity.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Tensile strength | 1.2 | MPa | CTM0137A |
| Elongation at break | 400 | % | CTM0137A |
| Modulus at 100% | 0.36 | MPa | CTM0137A |
| Hardness | 19 | Shore A | CTM0099 |