DOWSIL Q5-8401
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

Main features
- 24-Hour Pot Life at 25 deg C
- 90-Minute Cure at 120 deg C
- 830 psi Aluminum Lap Shear
Product Description
DOWSIL Q5-8401 Adhesive Kit is a two-part, 1:1 dark-gray silicone adhesive designed for heat-cure bonding and sealing. Part A and Part B have typical viscosities of 113,850 cP and 76,325 cP, while the mixed material is 77,425 cP. A 24-hour pot life at 25 deg C provides an extended processing window, followed by a typical heat cure of 90 minutes at 120 deg C. The cured adhesive reaches Shore A 61 hardness, 875 psi tensile strength, 210% elongation, and 830 psi lap shear on aluminum.
Key features
- 24-Hour Pot Life at 25 deg C: Typical pot life applies to the mixed adhesive before heat cure.
- 90-Minute Cure at 120 deg C: The listed heat-cure condition develops the cured silicone adhesive.
- 830 psi Aluminum Lap Shear: Typical cured elongation is 210%.
Applications
Sealing lids and housings; attaching baseplates; gasketing; connector sealing; engine controllers; ABS; transmission controllers.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Additional Information
As-supplied / before-processing properties
Typical processing values apply to the exact Q5-8401 Part A/Part B kit; component viscosities are shown separately.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Viscosity - Part A | 113,850 | cP | Typical; Part A |
| Viscosity - Part B | 76,325 | cP | Typical; Part B |
| Viscosity - mixed | 77,425 | cP | Typical; mixed material |
| Pot life | 24 | h | 25 deg C |
| Heat-cure schedule | 90 | min | 120 deg C |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Specific gravity | 1.31 | Typical cured material | |
| Tensile strength | 875 | psi | Typical cured material |
| Elongation | 210 | % | Typical cured material |
| Shore A hardness | 61 | Typical cured material | |
| Lap shear strength | 830 | psi | Aluminum substrate |