ELANTAS EA-02
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- 55 cP Hardener Viscosity
- Epoxy Potting Part B
- Electrical Insulation System Use
Product Description
CONACURE EA-02 Hardener is a modified aliphatic amine curing-agent component for epoxy potting and encapsulation systems. The amber liquid has a typical viscosity of 55 cP and specific gravity of 1.0 at 25 deg C. In the CONAPOXY DPFR-29589 system, EA-02 serves as Part B for electrical and electronic potting applications, including modules, transformers, coils, and strain-sensitive devices. Mix ratio and cured-system properties depend on the selected Part A resin. EA-02 is supplied as the hardener component, not as a complete epoxy system.
Key features
- Hardener Viscosity: The amber liquid has a typical viscosity of 55 cP at 25 deg C.
- Epoxy Potting Part B: EA-02 serves as the hardener component in selected two-component epoxy potting and encapsulation systems.
- Electrical Insulation System Use: In the DPFR-29589 system, applications include modules, transformers, coils, and strain-sensitive devices.
Applications
Electrical insulation; epoxy potting and encapsulation systems; modules; transformers; coils; strain-sensitive devices.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Typical EA-02 hardener-component values; no complete-system properties are included.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Viscosity | 55 | cP | Typical; 25 deg C |
| Specific gravity | 1.0 | - | Typical; 25 deg C |
| Color | Amber | - | Typical; as supplied |
| Flash point | >94 | deg C | ASTM D93 |