FREKOTE C-210
Harmonization Code : 3215907090 | Ink, whether or not concentrated or solid (excl. printing ink, printer/copier ink cartridges incorporating mechanical or electrical components, and solid ink in engineered shapes for printers/copiers)

Main features
- Above 60 deg C Hot-Mold Touch-Up
- Ready-to-Use No-Mix Emulsion
- Spray, Brush, Wipe, or Dip
Product Description
LOCTITE FREKOTE C-210 is a water-based mold release product for hot-mold touch-up and spray application over a LOCTITE FREKOTE C-200 base coat. It is intended for touch-up on molds above 60 deg C or where spray application is used. The product is supplied ready to use, requires no mixing, and provides multiple releases without contaminating transfer to molded parts. It is a white emulsion with typical specific gravity of 1.00; application methods include spray, brush, wipe, or dip.
Key features
- Hot-Mold Touch-Up: The product is intended for touch-up on molds above 60 deg C.
- Ready-to-Use No-Mix Emulsion: The product is a white water-based emulsion with typical specific gravity of 1.00 and requires no mixing.
- Spray, Brush, Wipe, or Dip: Spray is recommended for hot-mold touch-up; brush, wipe, and dip are alternative application methods.
Applications
Hot-mold touch-up; spray-applied mold release; use over a LOCTITE FREKOTE C-200 base coat.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Other Properties
Additional Information
As-supplied / before-processing properties
Typical C-210 as-supplied values from the manufacturer-authored C-200/C-210 product description sheet.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | White emulsion | - | As supplied |
| Odor | Slight mild | - | As supplied |
| Specific gravity | 1.00 | - | Typical C-210 value |
| Storage limit | Below 40 | deg C | Special caution in exact product sheet |