LINQCELL GDP310 | 310um Carbon Paper
Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

Main features
- 0.31 mm - 310 µm - 12.20 mil
- Customizable with PTFE Coating and Available in Roll Form
- Optimized as gas diffusion layers in fuel cells
Product Description
LINQCELL GDP310 is a 310-µm thick graphitized carbon fiber paper made from high-quality polyacrylonitrile (PAN) fibers. The fibers undergo a wet-laying process to form a non-woven, fibrous, and porous structure, which is then carbonized and graphitized at 1600 °C. This high-temperature graphitization results in high electrical conductivity, high oxidation resistance, and excellent thermal stability, making LINQCELL GDP310 highly recommended as gas diffusion layers in fuel cells. It can also be used as gas diffusion substrates for carbon dioxide electrolyzers.
Key Features:
- High-Temperature Graphitization: Graphitized at an elevated temperature of 1600 °C, this carbon fiber paper has a highly-crystalline graphite-like structure, enhancing conductivity, thermal stability, and oxidation resistance for demanding applications.
- No MPL and PTFE Layer: Enables direct control of interfacial modifications for system-specific optimization in fuel cells and electrochemical devices.
- High Permeability Despite Thickness ≥200 µm: Maintains high permeability for efficient gas diffusion and water management.
Highly Recommended As:
- Gas diffusion layers of fuel cells, particularly proton exchange membrane fuel cells
- Gas diffusion substrates of carbon dioxide electrolyzer electrodes
Due to the absence of a microporous layer, LINQCELL GDP310 exhibits high permeability despite its thickness (≥200 µm). This makes it particularly well-suited for high-humidity fuel cell operation (≥60%) at temperatures between 50 and 80 °C. In medium humidity conditions (20 to 60%), LINQCELL GDP310 may perform effectively, but the temperature should be kept low (≤50 °C).
Recommended For Fuel Cells Operating at:
- High humidity (≥60%) at temperatures between 50 to 80 °C
- Medium relative humidity (20 to 60%) at low temperatures ≤50 °C
LINQCELL GDP310 can be customized to meet specific requirements. It can be coated with a 10 wt% PTFE layer and is also available in roll form.