LOCTITE 190015
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

Main features
- No-Mix Anaerobic Bonding
- Flexible Cured Bond Profile
- Primer-Assisted Larger-Gap Bonding
Product Description
LOCTITE 190015 is a one-part red anaerobic acrylic adhesive for flexible bonding applications. The uncured material has a typical specific gravity of 1.18 and viscosity of 5,000 to 10,000 cP. The cured material combines Shore A hardness of 35 to 40 with the product's flexible bonding profile. Its no-mix format simplifies preparation, and primer-assisted use permits bonding across larger gaps. Applications include Red Explosive Charge Bonder assemblies and other bonding tasks that require a flexible anaerobic adhesive.
Key features
- One-part anaerobic format: The adhesive requires no component mixing before application.
- Flexible cured profile: Cured Shore A hardness is 35 to 40.
- Primer-assisted gap bonding: Primer supports use across larger bonding gaps.
Applications
Applications include Red Explosive Charge Bonder assemblies, flexible anaerobic bonding, and larger-gap bonding when used with primer.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Other Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Red | - | As supplied |
| Specific gravity | 1.18 | - | Typical; uncured material |
| Viscosity | 5,000 to 10,000 | cP | Typical; uncured material |