LOCTITE 5144H

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

LOCTITE 5144H

Main features

  • High-Viscosity Formulation
  • Fast Fixture Speed
  • Blue Color For Inspection

Product Description

LOCTITE 5144H is a high-viscosity ethyl cyanoacrylate adhesive formulated for bonding rubber substrates and other dissimilar or porous materials. This one-part, moisture-curing adhesive features a blue liquid appearance that supports visual quality control during application. Its viscosity helps accommodate small gaps, while its fast fixture speed on EPDM substrates can support efficient assembly processes. LOCTITE® 5144H™ develops functional bond strength rapidly and continues curing for up to 24 hours to achieve full chemical and solvent resistance.

Key features

  • High-viscosity formulation: Viscosity of 1,700–2,750 cP supports gap-filling applications and controlled dispensing.
  • Fast fixture speed: Achieves fixture time of ≤30 seconds on EPDM under test conditions.
  • Blue color for inspection: Facilitates visual quality verification during adhesive application.

Applications / Suitable for

  • Bonding EPDM and other rubber substrates
  • Joining dissimilar materials
  • Bonding porous materials
  • Assembly applications requiring rapid fixture times
Product Family

LOCTITE 5144H

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Blue liquid
Chemistry TypeChemistry Type
Ethyl cyanoacrylate
Physical Properties
ViscosityViscosity
1,700 to 2,750 mPa.s
Electrical Properties
Dielectric StrengthDielectric Strength
11.6 kV/mm
Other Properties
Storage TemperatureStorage Temperature
2 °C to 8 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the adhesive in its supplied state.

Property Value Unit Method / condition
Chemistry Ethyl cyanoacrylate — One-part adhesive
Appearance Blue liquid — Uncured state
Viscosity 1,700–2,750 cP 22°C, shear rate 100 s⁻¹
Fixture Time ≤30 seconds EPDM substrate
Storage Temperature 2–8 °C Recommended storage range
Technical properties

After-processing / final-state properties

Typical properties after 24 hours cure at 22°C.

Property Value Unit Method / condition
Tensile Strength 26 N/mm² ISO 6922, Aluminum-to-Aluminum
Softening Point 165 °C DIN EN 1427
Dielectric Breakdown Strength 11.6 kV/mm IEC 60243-1
Dielectric Constant 5.4 — IEC 60250, 1 kHz
Coefficient of Thermal Expansion 227 × 10⁻⁶ K⁻¹ 24-hour cure

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers