LOCTITE AA 3108
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Main features
- Fast UV-Cure Potting
- High-Elongation Cured Protection
- Dielectric Encapsulation Performance
Product Description
LOCTITE AA 3108 is a one-part, medium-viscosity UV-curing acrylated urethane/acrylic material for potting and sealing rigid assemblies. The translucent, colorless liquid is designed primarily for glass-to-metal joints and other dissimilar rigid substrates exposed to thermal cycling. On glass, fixture can be achieved in 15 seconds or less at 50 mW/cm^2 measured at 365 nm using a medium-pressure mercury arc light source. After a 30-second cure at 100 mW/cm^2 using an electrodeless D bulb, typical properties include 330% elongation, 7.91 N/mm^2 tensile strength, and 37 kV/mm dielectric breakdown strength. The flexible cured material is suitable for evaluation where electrical insulation is important; cure and bond performance depend on light intensity, wavelength, geometry, and substrate.
Key features
- Fast UV fixture: Glass reaches fixture strength in 15 seconds or less at 50 mW/cm^2 measured at 365 nm using a medium-pressure mercury arc light source.
- Cured elongation: Typical elongation at break is 330% after a 30-second cure at 100 mW/cm^2 using an electrodeless D bulb.
- Dielectric breakdown strength: Typical value is 37 kV/mm by IEC 60243-1 after a 30-second cure at 100 mW/cm^2 using an electrodeless D bulb.
Applications
Potting and sealing glass-to-metal joints and other dissimilar rigid substrates subject to thermal cycling.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Chemical Properties
Electrical Properties
Other Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Translucent colorless liquid | Uncured | |
| Specific gravity | 1.08 | 25 deg C | |
| Brookfield viscosity | 3,600 to 6,600 | mPa s (cP) | 25 deg C; RVT; spindle 4; 20 rpm |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Shore hardness | 72 minimum | Durometer A | ISO 868; cured 30 s at 100 mW/cm^2 using D bulb |
| Elongation at break | 330 | % | ISO 527-3; cured 30 s at 100 mW/cm^2 using D bulb |
| Tensile strength | 7.91 | N/mm^2 | ISO 527-3; cured 30 s at 100 mW/cm^2 using D bulb |
| Dielectric breakdown strength | 37 | kV/mm | IEC 60243-1; cured material |
| Glass-to-steel block shear | 3.5 | N/mm^2 | ISO 13445; 0.127 mm gap; 100 mW/cm^2 at 365 nm for 30 s; D bulb |