LOCTITE AA 331

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

LOCTITE AA 331

Main features

  • Rapid Activator-Assisted Fixture
  • High-Strength Metal Bonding
  • Magnet Assembly Impact Resistance

Product Description

LOCTITE AA 331 is a one-component, medium-viscosity modified acrylic structural adhesive for metal bonding, including permanent-magnet and electric-motor assemblies. The adhesive is supplied separately from LOCTITE SF 7387 activator, which is required for room-temperature cure. On grit-blasted mild steel with single-side activator, fixture is 17 seconds at a 0.05 mm gap and lap shear is 13.8 N/mm^2 after 24 hours at 23 deg C. The cured adhesive develops peel, impact, and magnet-bond strength; values depend on activator placement, bondline gap, surface preparation, and cure conditions.

Key features

  • Rapid activator-assisted fixture: Fixture is 17 seconds at a 0.05 mm gap on grit-blasted mild steel at 23 deg C with Activator 7387 on one side.
  • Steel lap shear strength: Lap shear is 13.8 N/mm^2 after 24 hours at 23 deg C on grit-blasted mild steel with a 0.05 mm gap and Activator 7387 on one side.
  • Ferrite-to-steel bond strength: Ferrite-to-mild-steel block shear is 12 N/mm^2 after 48 hours at 23 deg C with a 0.05 mm gap and Activator 7387 on both sides.

Applications

Metal-to-metal structural bonding, including DC motor/magnet bonding and precoated sheet-metal assemblies.

Product Family

LOCTITE AA 331

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Light yellow to sand yellow paste
Chemistry TypeChemistry Type
Modified acrylic
Specific GravitySpecific Gravity
1.08
Physical Properties
ViscosityViscosity
19,000 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
64 °C
Mechanical Properties
ElongationElongation
3.0 %
Chemical Properties
Water AbsorptionWater Absorption
0.78 %
Other Properties
Storage TemperatureStorage Temperature
8 °C to 21 °C

Additional Information

Technical properties

As-supplied / before-processing properties

The adhesive is the page entity; LOCTITE SF 7387 activator is separately supplied and required for the cited room-temperature cure process.

PropertyValueUnitMethod / condition
AppearanceLight yellow to sand yellow pasteUncured
Specific gravity1.0823 deg C
Cone and plate viscosity19,000mPa s25 deg C; PHYSICA MK22; 5 s^-1
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Glass transition temperature64deg CTMA; cured 48 h at 23 deg C plus 3 h at 80 deg C; tested at 23 deg C
Shore hardness86Durometer DISO 868; cured 48 h at 23 deg C plus 3 h at 80 deg C; tested at 23 deg C
Lap shear strength13.8N/mm^2ISO 4587; steel; 0.05 mm gap; Activator 7387 on one side; 24 h at 23 deg C
180 deg peel strength3.3N/mmISO 8510-2; grit-blasted steel
Ferrite-to-steel block shear12N/mm^2ISO 13445; 0.05 mm gap; Activator 7387 on two sides; 48 h at 23 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers