LOCTITE AA 3922

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LOCTITE AA3922

Main features

  • Second-Scale UV Fixture
  • Low-Viscosity Precision Bonding
  • UV-Fluorescent Bond Inspection

Product Description

LOCTITE AA 3922 is a low-viscosity UV/visible-light-curing adhesive for fast bonding of stress-sensitive plastics, glass, metal and ceramics. At 25 deg C its viscosity is 150 to 450 mPa s, and fixture can be reached within 10 seconds on glass at 6 mW/cm^2 measured at 365 nm. The material fluoresces under UV light, supporting visual inspection for adhesive presence. Typical cured properties include 135% elongation and 18 N/mm^2 tensile strength after 30 seconds per side at 100 mW/cm^2 and 365 nm using an electrodeless D bulb. It was specifically developed for stainless steel cannula-to-hub, syringe and lancet assemblies.

Key features

  • Rapid UV Fixture: Fixture on glass is 10 seconds or less at 6 mW/cm^2 measured at 365 nm.
  • Low-Viscosity Dispensing: Typical viscosity is 150 to 450 mPa s at 25 deg C and 1,000 s^-1.
  • UV-Fluorescent Inspection: The adhesive fluoresces under black light to aid inspection for adhesive presence.

Applications

Bonding stress-sensitive plastics, metal, glass and ceramics, including cannula, hub, syringe and lancet assemblies.

Product Family

LOCTITE AA 3922

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Transparent to hazy liquid
Chemistry TypeChemistry Type
UV acrylic
Specific GravitySpecific Gravity
1.04
Physical Properties
ViscosityViscosity
150 to 450 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
575 °C
Mechanical Properties
ElongationElongation
135 %
Chemical Properties
Water AbsorptionWater Absorption
7.2 %
Other Properties
Storage TemperatureStorage Temperature
8 °C to 21 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Specific gravity1.04Typical at 25 deg C
Viscosity150 to 450mPa sCone and plate; 25 deg C; shear rate 1,000 s^-1
UV fluorescencePositiveUncured material; black-light inspection feature
Fixture time10 maxsGlass; 6 mW/cm^2 measured at 365 nm; black-light source
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Glass transition temperature75deg CISO 11359-2; cured 100 mW/cm^2 at 365 nm for 30 s per side
Shore hardness66Shore DISO 868; cured 100 mW/cm^2 at 365 nm for 30 s per side
Elongation at break135%ISO 527-3; cured 100 mW/cm^2 at 365 nm for 30 s per side
Tensile strength18N/mm^2ISO 527-3; cured 100 mW/cm^2 at 365 nm for 30 s per side
Tensile modulus630N/mm^2ISO 527-3; cured 100 mW/cm^2 at 365 nm for 30 s per side
Block shear, polycarbonate to polycarbonate23.5N/mm^2Cured 100 mW/cm^2 at 365 nm for 30 s per side
Block shear, grit-blasted steel to glass15.0N/mm^2Cured 100 mW/cm^2 at 365 nm for 30 s per side
Block shear, grit-blasted aluminum to glass14.5N/mm^2Cured 100 mW/cm^2 at 365 nm for 30 s per side

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers