Main features

  • Fast Room-Temperature Fixture
  • Clear High-Peel Structural Bonds
  • 1:1 Static-Mix Processing

Product Description

LOCTITE AA H5004 is a two-part acrylic structural adhesive mixed 1:1 by volume for bonding plastics, metals, composites, FRP, stone, and ceramics. The medium-viscosity thixotropic system cures rapidly at room temperature when dispensed through a static mixer. At 25 deg C, gel time is 45 to 70 seconds and a fixture-strength threshold of 0.1 N/mm^2 is reached in 3 minutes or less on degreased, grit-blasted mild steel. The cured adhesive is virtually transparent, with Shore D 59 hardness, a typical Tg of 66 deg C, and high peel and impact strength. It is suited to assemblies where clear bondlines and fast handling are important.

Key features

  • Fast Room-Temperature Fixture: Develops 0.1 N/mm^2 fixture strength in 3 minutes or less at 25 deg C on degreased, grit-blasted mild steel.
  • Cured Bondline Transparency: The virtually transparent adhesive has Shore D 59 hardness and a typical Tg of 66 deg C.
  • High Peel and Impact Strength: The cured acrylic system resists peel, fatigue, and impact loading.

Applications

Structural bonding of plastics, metals, composites, FRP, stone, ceramics, steel, and aluminum.

Product Family

LOCTITE H5004

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry TypeChemistry Type
Acrylic
Component SystemComponent System
Two Part (Resin | Hardener)
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
66 °C
Mechanical Properties
ElongationElongation
5 %
Other Properties
Storage TemperatureStorage Temperature
8 °C to 21 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Part A and Part B values remain component-specific; the 1:1 mix ratio is by volume.

PropertyValueUnitMethod / condition
Mix ratio, Part A:Part B1:1-By volume
Specific gravity, Part A1.0-Typical; 25 deg C
Viscosity, Part A16,000 to 22,000mPa sLMS range; Brookfield RVF, 25 deg C, spindle 6, 10 rpm
Specific gravity, Part B1.0-Typical; 25 deg C
Viscosity, Part B15,000 to 21,000mPa sLMS range; Brookfield RVF, 25 deg C, spindle 5, 10 rpm
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Shore hardness59Durometer DTypical; ISO 868
Glass transition temperature66deg CTypical cured material
Tensile strength at break>=12N/mm^2LMS minimum; ISO 527-3
Tensile modulus600N/mm^2Typical; ISO 527-3
T-peel strength on aluminum>=4N/mmLMS minimum; ISO 11339, grit-blasted aluminum, cured >16 hours at 25 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers