LOCTITE PE3164

Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations

LOCTITE PE3164

Main features

  • 105 cP Hardener Viscosity
  • 2:1 PE 3140 Volume Mixing
  • 10 to 15 Minute System Work Time

Product Description

LOCTITE PE 3164 is the clear epoxy hardener component used as Part B with LOCTITE PE 3140 resin in a two-part potting system. As supplied, PE 3164 has 105 cP viscosity at 25 deg C using spindle 2 at 20 rpm and a specific gravity of 0.97. The PE 3140 and PE 3164 system mixes at 2:1 resin-to-hardener by volume and has a 10 to 15 minute work time for a 400 g mass at 25 deg C. Cure time is 16 hours at 25 deg C or 2 hours at 66 deg C.

Key features

  • 105 cP Hardener Viscosity: PE 3164 hardener viscosity is 105 cP at 25 deg C using spindle 2 at 20 rpm.
  • 2:1 PE 3140 Volume Mixing: The PE 3140 and PE 3164 system uses a 2:1 resin-to-hardener ratio by volume.
  • Paired-System Working Time: The PE 3140 and PE 3164 system has a 10 to 15 minute work time for a 400 g mass at 25 deg C.

Applications

Hardener component for the LOCTITE PE 3140 two-part potting system.

Product Family

LOCTITE PE3164

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Technical Specifications

General Properties
ColorColor
Clear
Specific GravitySpecific Gravity
0.96
Physical Properties
ViscosityViscosity
450 mPa.s

Additional Information

Technical properties

As supplied

Values apply to the LOCTITE PE 3164 hardener component only.

PropertyValueUnitMethod / condition
AppearanceClearPE 3164 hardener, as supplied
Viscosity105cPPE 3164 hardener; spindle 2, 20 rpm, 25 deg C
Specific gravity0.97PE 3164 hardener, as supplied
Storage temperature8 to 28deg CUnopened container unless otherwise labeled

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers