LORD 661/6

Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations

LORD 661/6

Main features

  • Up to 25.4 mm Gap Fill
  • 11-19 Minute Working Window at 32 deg C
  • 45-55 Minute Handling Strength

Product Description

LORD 661/Accelerator 6 is a two-part acrylic adhesive system for DCPD and modified-DCPD FRP and for cross-bonding those composites to metals. LORD 661 is a white to off-white paste with blue tint and typical viscosity of 125,000-350,000 cP. The system mixes 10:1 by volume or 7.4:1 by weight. At 32 deg C, LORD 661 has an 11-19 minute working time; handling strength is reached in 45-55 minutes, with 24-hour room-temperature cure. The mixed adhesive is non-sag and fills gaps up to 25.4 mm. This page refers specifically to Accelerator 6, not the separate 6GB variant.

Key features

  • Gap-Filling Capacity: The mixed system fills gaps up to 25.4 mm.
  • Mixed-System Work Time: LORD 661 mixed with Accelerator 6 has a typical working time of 11 to 19 minutes at 32 deg C.
  • Assembly Handling: The LORD 661 system reaches the stated handling-strength endpoint in 45 to 55 minutes.

Applications

DCPD and modified-DCPD FRP bonding and cross-bonding composites to metals.

Product Family

LORD 661/6

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
White/Off-white/Blue Tint Paste
DensityDensity
1055 -1174 kg/m3
Mix RatioMix Ratio
10:1
SolidsSolids
100 %
Physical Properties
ViscosityViscosity
125,000 - 350,000 mPa.s
Thermal Properties
Flash PointFlash Point
15 °C

Additional Information

Technical properties

As-supplied / before-processing properties

LORD 661 values and mixed-system values apply specifically to the LORD 661/Accelerator 6 system, not Accelerator 6GB.

PropertyValueUnitMethod / condition
LORD 661 viscosity125,000-350,000cPTypical
LORD 661 density1,055-1,174kg/m3Typical
Flash point15deg CTypical; LORD 661 component
Mix ratio10:1by volumeLORD 661 adhesive to Accelerator 6
Mix ratio7.4:1by weightLORD 661 adhesive to Accelerator 6
Solids content100%Typical; mixed system
Working time11-19minutesTypical; 1 in diameter bead at 32 deg C
Time to handling strength45-55minutesTypical; 100 psi lap-shear endpoint, 30 mil x 1 in x 1 in

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF