PERMABOND HL138

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

PERMABOND HL138

Main features

  • Low-Viscosity Retention for Close Clearances
  • Press-Fit and Clearance-Fit Shaft-Hub Assembly
  • Rapid 10-Minute Handling on Steel

Product Description

Permabond HL138 is a low-viscosity anaerobic retaining compound for shaft-hub assemblies, press fits and clearance-fit cylindrical metal parts. Its 150-300 cP viscosity at 25 deg C allows the liquid to flow into close clearances before curing when confined between mating metal surfaces. The product fills gaps up to 0.127 mm and reaches typical handling strength on M10 steel in 10 minutes at 23 deg C. Typical cured shear strength is 16 MPa on a steel collar-and-pin test to ISO 10123. HL138 fits close-clearance cylindrical retention where low viscosity and rapid handling are important.

Key features

  • Press- and clearance-fit retention: Retains shaft-hub and other close-fitting cylindrical metal assemblies.
  • Low-viscosity application: Viscosity is 150-300 cP at 25 deg C for flow into close clearances.
  • 10-minute handling on steel: Typical handling strength is reached on M10 steel in 10 minutes at 23 deg C.

Applications

Retaining shaft-hub assemblies; press fits; clearance fits and other close-fitting cylindrical metal parts.

Product Family

PERMABOND HL138

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Green
Chemistry TypeChemistry Type
Acrylic
Specific GravitySpecific Gravity
1.1
Physical Properties
ViscosityViscosity
150-300 mPa.s
Electrical Properties
Dielectric StrengthDielectric Strength
11 kV/mm
Thermal Properties
Thermal ConductivityThermal Conductivity
0.19 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Chemical compositionAcrylic-Uncured material
Viscosity150-300cPUncured material; 25 deg C
Specific gravity1.1-Uncured material
Storage temperature5 to 25deg CManufacturer storage guidance
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Break torque20N mTypical cured material; M10 steel; ISO 10964
Prevailing torque36N mTypical cured material; M10 steel; ISO 10964
Shear strength16MPaTypical cured material; steel collar and pin; ISO 10123

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF