PERMABOND UV670

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

PERMABOND UV670

Main features

  • Flexible Glass-to-Metal UV Bonding
  • Fast LED Fixture for Flexible Joints
  • High-Elongation Cured Adhesive

Product Description

Permabond UV670 is a single-part flexible UV-curable adhesive for glass-to-metal, metal and metalized-plastic assemblies. The methacrylate ester adhesive has a viscosity of 2,000-3,000 cP at 25 deg C and cures across 365-400 nm. Typical fixture is 2 seconds under a 100 mW/cm2 LED source; cure time depends on lamp output, distance and substrate transmission. After cure, typical steel-to-glass tensile strength is 6-10 N/mm2, tensile strength is 12 N/mm2 and elongation exceeds 80%. UV670 is used for flexible glass-to-metal and metalized-plastic joints.

Key features

  • Flexible glass-to-metal UV bonding: The cured adhesive combines >80% elongation with steel-to-glass tensile strength of 6-10 N/mm2.
  • Fast 2-second UV fixture: Typical fixture is 2 seconds under a 100 mW/cm2 LED source; actual cure time depends on the UV setup and substrate transmission.
  • 2,000-3,000 cP viscosity: The single-part adhesive has a typical viscosity of 2,000-3,000 cP at 25 deg C.

Applications

Metal-to-glass bonding; bonding metal and metalized plastics; flexible glass-to-metal assemblies.

Product Family

PERMABOND UV670

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Colourless, clear
Chemistry TypeChemistry Type
Methacrylate ester
Refractive indexRefractive index
1.490
Specific GravitySpecific Gravity
1.1
Physical Properties
ViscosityViscosity
2,000-3,000 mPa.s
Mechanical Properties
ElongationElongation
80 %

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Chemical compositionMethacrylate ester-Uncured adhesive
AppearanceColorless, clear-Uncured adhesive
Viscosity at 20 rpm2,000-3,000cP25 deg C
Specific gravity1.1-Uncured adhesive
Cure wavelength365-400nmUV cure
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Steel-to-glass tensile strength6-10N/mm2Typical cured joint; ASTM D-2095-69
Tensile strength12N/mm2Typical cured adhesive; ISO 37
Elongation>80%Typical cured adhesive; ISO 37
Hardness50-60Shore DTypical cured adhesive; ISO 868

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers