PLEXUS MA2030

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

PLEXUS MA2030

Main features

  • 30-32 Minute Work Time
  • 0.75-38 mm Structural Gaps
  • 90-125% Cured Elongation

Product Description

Plexus MA2030 White is a two-part 10:1 methacrylate structural adhesive for thermoplastic, metal and composite assemblies with an extended assembly window. At 23.9 deg C, typical work time is 30-32 minutes. The adhesive fills gaps from 0.75 to 38 mm, with final gap capability dependent on laminate thickness and composition. After cure, typical tensile strength is 20.7-23.4 MPa, tensile modulus is 621-827 MPa and elongation at break is 90-125%. Typical aluminum lap-shear strength is 12.4 MPa.

Key features

  • 30-32 minute work time: Typical work time is 30-32 minutes at 23.9 deg C.
  • Structural gaps from 0.75 to 38 mm: The adhesive fills gaps from 0.75 to 38 mm, subject to laminate thickness and composition.
  • 90-125% cured elongation: Typical elongation at break is 90-125%, with tensile strength of 20.7-23.4 MPa.

Applications

Structural bonding of thermoplastics, metals and composites; composite bonding in marine and transportation assemblies.

Product Family

PLEXUS MA2030

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Off-White/(Blue/Black)
Density (g)Density (g)
0.94/1.07 g/cm3
Mix RatioMix Ratio
10:1
Physical Properties
Viscosity (Part A)Viscosity (Part A)
180 - 220 mPa.s
Viscosity (Part B)Viscosity (Part B)
35 - 70 mPa.s
Mechanical Properties
ElongationElongation
90 - 125 %

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Part A viscosity180,000-220,000cPUncured adhesive
Part B viscosity35,000-70,000cPUncured activator
Part A density0.94g/mlUncured adhesive
Part B density1.07g/mlUncured activator
Mix ratio by volume10:1-Part A : Part B
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Tensile strength20.7-23.4MPaTypical cured adhesive; ISO 527
Tensile modulus621-827MPaTypical cured adhesive; ISO 527
Elongation at break90-125%Typical cured adhesive; ISO 527
Lap-shear strength12.4MPaTypical cured joint; aluminum; ASTM D1002

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers